drying kiln

Basic principles of wood drying

Like other natural plants, wood is also a hygroscopic material that exchanges moisture with the air. Various wood drying methods have common principles and principles that should be followed. The principle of wood drying is to use the difference in water absorption of the microcapillary system in the wood cell wall caused by the moisture content gradient (i.e. the difference between the surface moisture content and the internal moisture content) and the water vapor partial pressure difference formed after heating to promote the movement of water from the inside to the outside in both liquid and vapor states.

The process of wood drying is closely related to the climatic conditions around the wood. As we all know, felled wood will always get a certain degree of drying by itself, but the speed, degree and quality of drying are different in different regions and seasons. That is to say, the natural environment can also dry wood to a certain extent. However, natural drying generally takes a long time, and because no control is applied, the drying quality is difficult to meet the requirements.

The drying speed of wood can be greatly improved by placing wood in a drying kiln by artificial methods and using forced air circulation in a high temperature environment. If the drying kiln can maintain a suitable environment through effective measurement and control during the drying process, so that the internal moisture movement rate of the wood is coordinated with the surface moisture evaporation rate, and the wood is dried evenly from the outside to the inside, the wood can be dried quickly while ensuring the quality of wood drying.

drying kiln

Wood Drying Process

The complete wood drying process is divided into heating, preheating, drying, intermediate treatment, final treatment and cooling stages. Among them, the drying stage is the main stage for achieving wood drying and the longest stage. The evaporation of moisture contained in the wood mainly occurs in this stage.

Heating Stage

Heating refers to the slow increase of the temperature of the wood to a certain temperature value before preheating. On the one hand, the temperature of the core layer and the surface layer of the wood tends to be consistent; on the other hand, the shell is preheated to increase the temperature of the drying chamber to prevent condensation water from being generated in the early stage of drying or preheating stage, which is especially necessary for the heating stage in cold weather. In order to avoid excessive evaporation of moisture on the wood surface at this stage, the heating rate should not be too fast. The heating rate depends on the type, thickness and moisture content of the wood.

Preheating stage

The purpose of the preheating stage is to make the temperature gradient (temperature difference) and moisture content gradient (moisture content difference) of the wood along the thickness direction approach zero under a certain temperature and humidity environment, so as to create conditions for the wood to enter the moisture evaporation (drying) stage. The temperature and humidity environment in the preheating stage should make the wood basically not evaporate moisture in this stage, and also allow the surface of the wood to absorb moisture to a certain extent.

drying kiln

Drying stage

The drying stage is divided into the early drying stage and the late drying stage, also known as the uniform drying stage and the deceleration drying stage. When the moisture content of the wood is above the fiber saturation point, when the temperature, humidity and wind speed of the medium are certain, the free water in the wood will move along the large capillary system to the surface of the wood and evaporate from the surface of the wood. At this time, the evaporation of water is basically uniform, which is the uniform drying stage. When the free water evaporates, the absorbed water begins to move and evaporate. As the absorbed water continues to decrease, the energy required for water evaporation increases, and the rate of decrease in moisture content slows down. Therefore, when the wood is below the fiber saturation point, it is the deceleration drying stage.

Heating Stage

The drying stage is divided into the early drying stage and the late drying stage, also known as the uniform drying stage and the deceleration drying stage. When the moisture content of the wood is above the fiber saturation point, when the temperature, humidity and wind speed of the medium are certain, the free water in the wood will move along the large capillary system to the surface of the wood and evaporate from the surface of the wood. At this time, the evaporation of water is basically uniform, which is the uniform drying stage. When the free water evaporates, the absorbed water begins to move and evaporate. As the absorbed water continues to decrease, the energy required for water evaporation increases, and the rate of decrease in moisture content slows down. Therefore, when the wood is below the fiber saturation point, it is the deceleration drying stage.

Intermediate treatment stage

The drying stage is divided into the early drying stage and the late drying stage, also known as the uniform drying stage and the deceleration drying stage. When the moisture content of the wood is above the fiber saturation point, when the temperature, humidity and wind speed of the medium are certain, the free water in the wood will move along the large capillary system to the surface of the wood and evaporate from the surface of the wood. At this time, the evaporation of water is basically uniform, which is the uniform drying stage. When the free water evaporates, the absorbed water begins to move and evaporate. As the absorbed water continues to decrease, the energy required for water evaporation increases, and the rate of decrease in moisture content slows down. Therefore, when the wood is below the fiber saturation point, it is the deceleration drying stage.

lumber kiln

Heating Stage

When the wood is dried to the point where the moisture content drops to near the fiber saturation point, or because the evaporation intensity of the moisture on the wood surface is too high, the wood will produce a certain drying stress. At this time, appropriate intermediate treatment should be carried out. In the intermediate treatment stage, the evaporation of the wood moisture is temporarily stopped, and the wood is sprayed with steam to reduce the moisture content gradient of the wood along the thickness direction, thereby reducing the drying stress of the wood and improving the drying quality. The intensity of the intermediate treatment depends on the thickness and the magnitude of the stress generated at that time.

Final treatment and cooling stage

Treatment: When the wood is dried to the final moisture content requirement, in order to further reduce the moisture content gradient of the wood along the thickness direction and eliminate or reduce the stress generated during the drying process, a final treatment must be carried out. The humidity environment (equilibrium moisture content) of the final treatment is consistent with the equilibrium moisture content corresponding to the final moisture content.

Cooling: Similar to the heating stage, when the wood reaches the final moisture content requirement and undergoes appropriate final treatment, in order to avoid residual stress caused by a sharp drop in temperature, the wood must undergo a cooling process at an appropriate speed before leaving the kiln.

Get In Touch With Us