Wood drying typically refers to the process of removing moisture from wood through evaporation or boiling under the action of heat energy.
To remove moisture from wood, there must be a source of heat energy in its surrounding environment, which is generally the heat source generating the heat. At a certain temperature, moisture within the wood evaporates or boils off into the surrounding air, resulting in dried wood. When the moisture content in the wood drops to a certain level, we can use it to process and manufacture the products we need.
What Factors Affect Wood Drying?
1. External Factors
Temperature
Temperature is the primary factor influencing wood drying speed. As temperature increases, the vapor pressure of water within the wood rises, and the viscosity of liquid free water decreases, facilitating the movement and diffusion of moisture within the wood. The moisture-holding capacity of the drying medium increases, accelerating the evaporation rate of moisture from the wood surface. However, it’s important to note that excessively high temperatures can cause cracking, deformation, reduced mechanical strength, discoloration, etc., and should be appropriately controlled.Humidity
Relative humidity is a crucial factor affecting wood drying speed. At the same temperature and air velocity, higher relative humidity means higher water vapor partial pressure in the medium, making it harder for surface moisture to evaporate into the medium, thus slowing drying. Lower relative humidity speeds up surface evaporation, reduces surface moisture content, increases the moisture gradient, enhances internal moisture diffusion, and accelerates drying. However, excessively low relative humidity can cause or exacerbate drying defects such as cracking and honeycombing.Air Circulation Velocity
Air circulation velocity is another factor influencing wood drying speed. High-velocity air can disrupt the saturated vapor boundary layer on the wood surface, thereby improving heat and mass transfer conditions between the medium and the wood, speeding up drying. For refractory woods or when wood moisture content is low, the movement of internal moisture dictates the drying rate. Increasing air velocity to accelerate surface evaporation becomes ineffective and can instead increase the moisture gradient, raising the risk of drying defects. Therefore, refractory woods do not require very high air circulation velocities.

2. Internal Factors
Wood Species and Structural Characteristics
Different wood species have distinct structures. The size and number of pits, as well as the size of micropores in pit membranes, vary significantly. Consequently, the ease of moisture movement along these pathways differs, meaning wood species is a major internal factor affecting drying speed. Ring-porous hardwoods (e.g., Rosewood) have more occlusions in vessels and pits and smaller micropores in pit membranes, resulting in significantly slower drying speeds compared to diffuse-porous hardwoods. Within the same species, increased density raises resistance to moisture flow in large capillaries and lengthens the diffusion path through cell walls, making drying more difficult.Wood Thickness
Conventional wood drying can be approximated as a one-dimensional heat and mass transfer process along the thickness direction. Increased thickness lengthens the heat and mass transfer distance and increases resistance, significantly reducing drying speed.Wood Moisture Content
Below the fiber saturation point (FSP), as moisture content decreases, the transverse diffusion coefficient of bound water decreases, while the diffusion coefficient of water vapor in the cell lumens increases. However, since water vapor diffusion in lumens contributes little to the overall drying process, and lower moisture content means longer diffusion paths, drying becomes progressively more difficult as moisture content decreases.Heartwood vs. Sapwood
Heartwood cells in hardwoods contain more extractives, and pits in softwood heartwood are often occluded. Therefore, heartwood is generally more difficult to dry than sapwood.Wood Grain Direction
Wood rays facilitate moisture conduction. Radial moisture conduction is approximately 15%–20% greater than tangential conduction. Consequently, flat-sawn (tangential) boards usually dry faster than quarter-sawn (radial) boards.
Causes and solutions for cracking during wood drying
Wood cracking has the following forms: surface cracking, internal cracking, end cracking and wheel cracking.
Let’s briefly understand the causes of these cracking forms:
- Surface cracking
Refers to surface cracks. Surface cracks refer to cracks on the surface of the log body or finished timber. Cracks are usually limited to the tangent plane and develop radially. When wood is dried, water evaporates from the surface first. When the moisture content of the surface layer drops below the fiber saturation point, the surface wood begins to shrink, but at this time the moisture content of the adjacent inner layer of wood is still above the fiber saturation point and does not shrink. The shrinkage of the surface wood is restricted by the inner layer of wood and cannot shrink freely, thus generating internal stress in the wood: the surface wood is under tension and the inner layer is under compression. The more severe the drying conditions, the greater the difference in moisture content between the inner and outer layers of wood, and the greater the internal stress generated. If the tensile stress of the surface exceeds the tensile strength of the wood’s transverse grain, the wood tissue is torn. Since the tensile strength of the tissue along the wood ray is lower than that of the adjacent wood fibers, cracks first occur along the wood ray.

- Internal cracks
That is, internal cracks. Internal cracks are also often called honeycomb cracks. Internal cracks occur in the late stage of drying, and sometimes in the storage period of dried materials. It is usually not easy to find from the outside of the wood, but in severe cases, it can be judged by the depression of the wood surface. Internal cracks are caused by tensile stress in the inner layer of wood.

- End cracks
That is, end cracks. End cracks are either limited to the end of the wood, or extend to one or both sides of the end, the latter of which is usually called splitting. The main reason is that the water conductivity of the wood along the grain direction is much greater than that in the transverse direction. When the wood is dry, the water evaporates much faster from the end than from the side. The moisture content of the end is lower than that of the middle part, and the shrinkage of the end is limited by the wood in the middle, so tensile (stretching) stress is generated at the end. When the tensile stress exceeds the tensile strength of the wood across the grain, the end cracks.

- Ring cracks
This type of crack develops along the growth ring direction and often extends to several adjacent growth rings. Ring cracks usually occur in the early stage of drying and appear on the end of the wood. As the drying progresses, the cracks deepen and lengthen. Sometimes it occurs inside, but it appears in the late stage of drying, which is caused by severe internal tensile stress.

Countermeasures
Apply High-Temperature Conditioning
To reduce internal checking, high-temperature conditioning can be used. The tensile residual strain on the wood surface causing internal checks can be eliminated by subjecting the wood to high temperature and high humidity towards the end of the drying schedule. During this treatment, surface wetting causes expansion, creating compressive residual strain that counteracts the original tensile residual strain, thereby eliminating internal checks.Mechanical Restraint
Use mechanical methods to forcibly restrain wood from expanding and shrinking, such as wiring the ends of dried lumber, using end caps (anti-check rings), or applying clamp boards (combination nail plates). This can also help prevent cracking.Apply Water-Repellent Coatings
Applying water-repellent coatings to the ends and surfaces of lumber slows down the evaporation rate from the surface. This reduces the moisture gradient within the wood and consequently reduces cracking.Treat with Water-Repellent Preservatives by Pressure Impregnation
A more effective method is pressure impregnation treatment with water-repellent preservatives, forcing the agent deep into the wood to achieve long-lasting crack prevention.Optimize Sawing Methods During Milling
Due to wood’s anisotropy, under the same temperature and humidity changes, tangential shrinkage/swelling is the greatest, followed by radial, with longitudinal changes being the smallest. Therefore, producing more quarter-sawn (radial) boards during sawing can reduce cracking. Boards containing the pith are particularly prone to severe splitting during drying due to the difference in radial and tangential shrinkage near the pith. The best approach during milling is to avoid producing boards containing the pith.